Silicone compound as above XR-j plus additional hardening of the top surface to facilitate handling and installation during complex assemblies.
Properties | Unit | XR-j | Test method | Specimen |
---|---|---|---|---|
Color | - | Light Gray | Visual | - |
Specific Gravity | - | 3.2 | ASTM D792 | A |
Hardness Highest Value | Shore OO | 80 | ASTM D2240 | B |
Tensile Strength | MPa (psi) | 0.2 (29.0) | ASTM D412 | A |
Elongation | % | 25 | ASTM D412 | A |
Elongation | N/mm (ppi) | 1.0 (5.7) | ASTM D624 | A |
Properties | Unit | XR-j | Test method | Specimen |
---|---|---|---|---|
Volume Resistivity | Ohm-m | 1.0x10¹¹ | ASTM D257 | C |
Breakdown Voltage | kV/mm (volts/mil) | 18 (457) | ASTM D149 | C |
Dielectric Strength | kV/mm (volts/mil) | 13 (330) | ASTM D149 | C |
Dielectric Constant | 50Hz, 1kHz, 1MHz | 6.8, 6.8, 6.8 | ASTM D150 | A |
Dissipation Factor | 50Hz, 1kHz, 1MHz | 0.006, 0.001, 0.001 | ASTM D150 | A |
Properties | Unit | XR-j | Test method | Specimen |
---|---|---|---|---|
Thermal Conductivity | W/m-K | 14.0 by ASTM D5470, 9.0 by Hot Disk | ASTM D5470*1, ISO/CD 22007-2 | - |
Useful Temperature | ℃ (°F) | -40 to +150 (-40 to +302) | - | - |
Low molecular Siloxane | wt% | D4 to D20 Total, 0.0020 or less | Gas Chromatography | - |
Flame Retardant | - | V-0 | UL 94 | - |
Materials Direct
Precision cut technical materials fast
We’re available to assist you for your next project
A division of Universal Science UK
www.universal-science.com
Reviews
There are no reviews yet.